Universal Wire Works 182 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 182 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 182 is used for arc welding Inconel types 600 and 601 to themselves or one to another. Deposited weld metal meets the most stringent radiographic requirements. Alloy 182 dissimilar welding applications are: joining Monel type 400 to carbon steel; stainless steel to carbon steel; and Inconel type alloy 600 and Incoloy type alloy 800 to Nickel 200, Monel type alloy 400, carbon steel and stainless and Nickel 200 to stainless. Alloy 182 typical applications include welding ASTM B163, B166, B167, and B168. Electrode sizes 3/32 and 1/8 diameters can be used in all positions while the larger 5/32 and 3/16 diameters are used in the flat and horizontal positions.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 13 - 17 %
13 - 17 %
Cobalt, Co <= 0.12 %
<= 0.12 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 10 %
<= 10 %
Manganese, Mn 5.0 - 9.5 %
5.0 - 9.5 %
Nickel, Ni >= 59 %
>= 59 %
Niobium, Nb (Columbium, Cb) 1.0 - 2.5 %
1.0 - 2.5 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.015 %
<= 0.015 %
Tantalum, Ta <= 0.30 %
<= 0.30 %
Titanium, Ti <= 1.0 %
<= 1.0 %