Universal Wire Works 317L Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 317L Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Universal 317L electrodes are slightly higher in alloy content than type 316L, particularly in molybdenum and are used primarily for welding type 317 stainless steel. This electrode is used extensively for resistance to corrosion caused by sulfuric and sulfurous acids. Alloy 317L is used in the manufacturing and maintenance repair of equipment and parts for the chemical, refining, paper and textile industries. Allow 317L can be used to fabricate equipment subject to temperatures up to 1300 degrees F.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 607 MPa
88000 psi
Elongation at Break 38 %
38 %
Component Elements Properties Metric English Comments
Carbon, C 0.030 %
0.030 %
Chromium, Cr 19.8 %
19.8 %
Iron, Fe 61.9 %
61.9 %
As Remainder
Manganese, Mn 1.8 %
1.8 %
Molybdenum, Mo 3.25 %
3.25 %
Nickel, Ni 12.6 %
12.6 %
Silicon, Si 0.60 %
0.60 %