Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode

Category Metal , Ferrous Metal , Carbon Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multiple pass welding have a spray-like transfer with very little spatter. The fast freezing slag facilitates welding in all positions and is easily removed. Alloy 81T1-Ni1 is formulated for welding ASTM A572, A302, A588, and A734. These steels are used in the fabrication of transmission poles, light poles, earth moving and mining machinery and offshore platforms. Alloy 81T1-Ni2 is formulated for welding ASTM A572, A575, and A734. The combination of strength and CVN toughness of Ni-2 make it ideal for applications such as offshore platform construction, shipbuilding, earthmoving and mining equipment.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 621 MPa
90000 psi
Tensile Strength, Yield 552 MPa
80000 psi
Elongation at Break 22 %
22 %
Charpy Impact 40.7 J

@Temperature -40.0 °C
30.0 ft-lb

@Temperature -40.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Iron, Fe 96.1 %
96.1 %
As remainder
Manganese, Mn 0.90 %
0.90 %
Nickel, Ni 2.4 %
2.4 %
Phosphorous, P 0.14 %
0.14 %
Silicon, Si 0.30 %
0.30 %
Sulfur, S 0.14 %
0.14 %
Users viewing this material also viewed the following: