Wellman Wellamid® XT1573-N Impact Modified Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® XT1573-N Impact Modified Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Impact Modified Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0158 - 0.0198 cm/cm
0.0158 - 0.0198 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0199 - 0.0239 cm/cm
0.0199 - 0.0239 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-93
Elongation at Break 65 %
65 %
ISO 527-93
Flexural Strength 73.0 MPa
10600 psi
ISO 178-93
Flexural Modulus 1.925 GPa
279.2 ksi
ISO 178-93
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-93