Wieland 1023 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1023 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental
Physical Properties Metric English Comments
Density 10.7 g/cc
0.387 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 110
110
HV5; glowed
Tensile Strength, Ultimate 420 MPa
60900 psi
Elongation at Break 35 %
35 %
Thermal Properties Metric English Comments
Melting Point 820 - 910 °C
1510 - 1670 °F
Solidus 820 °C
1510 °F
Liquidus 910 °C
1670 °F
Component Elements Properties Metric English Comments
Copper, Cu 46.7 %
46.7 %
Gold, Au 33.3 %
33.3 %
Silver, Ag 9.0 %
9.0 %
Zinc, Zn 11 %
11 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1010 - 1110 °C
1850 - 2030 °F
Descriptive Properties Value Comments
Color yellow