Wieland 1751 Wilaform Palladium

Category Metal , Nonferrous Metal , Precious Metal , Palladium Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1751 Wilaform Palladium.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Approach-steady palladium alloy for nearly all purposes in decoration manufacturingApplications: casting, chains, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 11.0 g/cc
0.397 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 130
130
HV5; glowed
Thermal Properties Metric English Comments
Melting Point 1150 - 1220 °C
2100 - 2230 °F
Solidus 1150 °C
2100 °F
Liquidus 1220 °C
2230 °F
Component Elements Properties Metric English Comments
Copper, Cu 10 %
10 %
Palladium, Pd 50 %
50 %
Silver, Ag 40 %
40 %
Processing Properties Metric English Comments
Processing Temperature 800.0 °C
1472 °F
Cuvette Temp
Casting Temperature 1320 - 1420 °C
2410 - 2590 °F
Descriptive Properties Value Comments
Color grey