Wieland 1757 Wilaform Platinum

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1757 Wilaform Platinum.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Platinum alloy without nickel, low-priced for all kinds of decoration productionApplications: chains, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 21.5 g/cc
0.777 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 160
160
HV5; glowed
Thermal Properties Metric English Comments
Melting Point 1800 - 1820 °C
3270 - 3310 °F
Solidus 1800 °C
3270 °F
Liquidus 1820 °C
3310 °F
Component Elements Properties Metric English Comments
Iridium, Ir 15 %
15 %
Platinum, Pt 85 %
85 %
Processing Properties Metric English Comments
Casting Temperature 1950 - 2150 °C
3540 - 3900 °F
Descriptive Properties Value Comments
Color platinum-white