| Category | Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Silver Alloy |
| Manufacturer | Wieland |
| Trade Name | Auropal |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Wieland Auropal 50 Casting Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 13.4 g/cc | 0.484 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 270 | 270 | HV5/30; as cast |
| 270 | 270 | HV5/30; hardened | |
| Tensile Strength, Yield | 689.96 MPa @Strain 0.200 % |
100070 psi @Strain 0.200 % |
as cast |
| 729.95 MPa @Strain 0.200 % |
105870 psi @Strain 0.200 % |
hardened | |
| Elongation at Break | 6.0 % | 6.0 % | as cast |
| 8.0 % | 8.0 % | hardened | |
| Modulus of Elasticity | 104 GPa | 15100 ksi |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 12 % | 12 % | |
| Gold, Au | 50 % | 50 % | |
| Palladium, Pd | 4.9 % | 4.9 % | |
| Silver, Ag | 32 % | 32 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 699 °C | 1290 °F | Preheating Temp. |
| Melt Temperature | 849 - 910 °C | 1560 - 1670 °F | |
| Casting Temperature | 1100 °C | 2010 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | yellow |