Zoltek Panex 30® Graphitized Spun Yarn Carbon Fabric

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 30®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 30® Graphitized Spun Yarn Carbon Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Graphitized Spun Yarn Carbon FabricApplications include: Fuel Cells Diffusion Layers, Low Cost Carbon-Carbon Materials, Efficient Chemical Vapor Filtration
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
Thickness 381 microns
15.0 mil
660 microns
26.0 mil
1016 microns
40.00 mil
Component Elements Properties Metric English Comments
Carbon, C 99 %
99 %
Descriptive Properties Value Comments
Areal Weights, g/m2 115
237
288
Roll Length, m 36
73
Width, mm 1067
838
Yarn Input 2/10
2/27