Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® FXC810FE PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810FE is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ferrite colour effects. The colour package may effect performance.This data was supp.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable Information provided by Polykemi AB |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
Plaskolite Optix® PL-150 Acrylic Resin
(discontinued **) Injection/extrusion pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 215 W1 902176 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, weather-stabilized |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Lucite International Diakon® CLG902LX Acrylic Polymer Information provided by Lucite International |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 2781 |
Lubrizol Advanced Materials Pearlstick® D40-70/14 Linear Thermoplastic Polyurethane Pearlstick D40-70/14 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. .. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA4/6 HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS LNP THERMOCOMP* NF001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183-87 |
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6 Description: Abrasion Resistant Nylon 6Information provided by Wellman. |
|||
Density | 1.18 g/cc @Temperature 23.0 °C |
0.0426 lb/in³ @Temperature 73.4 °F |
ASTM D1928 |
Trelleborg Horda Cable E8551 Strippable Semiconductive Shielding E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
DSM Stanyl® TW341 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0334G5M25CL Glass/Mineral Reinforced Coupled |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D792 |
BASF Elastollan® C-78A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, General Description
(discontinu Product form is white, odorless chips. Distinguishing Feature: Medium polymer viscosity. Versatile.35 % Chlorine Content. 1% Sulfur Content. Excellent Abrasion Resistance. Excellent Chemical Re.. |
|||
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |