Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.22 g/cc | 0.0441 lb/in³ | |
Plastcom SLOVAMID 66 T 15 MI PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling and impact modified. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produc.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6) PENNITE® 4512 is a 12% glass fiber reinforced, black pigmented, thermally modified, type 6 nylon, available in sheets and rolls for high performance thermoforming and fabrication applications. PENN.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO data |
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | |
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)< Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be .. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 2781 |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DX04462C PC LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/12 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 50% Filler by WeightAppearance: Black and Natural ColorTPCI# 9814104Information provided by TP Composites, .. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
Stir SpA C 2012 65 AT (PVC) Application: Molding for treadInformation provided by STIR SpA |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PC/PBT IM 1799 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | DIN 53479 |
Polyram RamOfin PPH300J8 Polypropylene, 40% Glass Fiber 40% glass fiber and glass beads reinforced, high stiffness polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
Chengdu Polyster CH7563 Thermoplastic Polyether-ester Elastomer (TPEE) Poly-basic block copolymer. Good compatibility with PBT, PET and PA. For blending with PBT, PET and PA to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
Chengdu Polyster H7560 Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, wires, cables and optical fiber, ho.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30 Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | |
Dow PAPI™ 901 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a high functionality and a high viscosity resulting in highly rigid foams. This product is desi.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
DSM Arnite® B604T PBT-I |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 7010/K Flexible PVC, Lead Free Pipes |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | |
BASF Lupranate® 265 Isocyanate Description: Lupranate® 265 Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate 265 Isocyanate is used in the i.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | |
BASF Lupranate® M Isocyanate Description: Lupranate® M Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate M Isocyanate is used in the isoc.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
BASF Elastollan® 690A15N Polyester Type Polyurethane Elastomer This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes.. |
|||
Density | 1.22 g/cc | 0.0441 lb/in³ | |
BASF Lupranate® 5143 Isocyanate Description: Lupranate® 5143 isocyanate is a liquid, carbodiimide-modified 4,4’-diphenylmethane diisocyanate. With manufacturing advances, Lupranate 5143 isocyanate achieves better low temperature.. |