Physical Properties Metric English Comments
Density 2.55 g/cc
0.0921 lb/in³
Apparent
Gouda Vuurvast AK 60 A Dense Refractory Brick
Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% ..
Density 2.55 g/cc
0.0921 lb/in³
Apparent
Gouda Vuurvast AK 60 AP Dense Refractory Brick
Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime ..
Density 2.55 g/cc
0.0921 lb/in³
Apparent
Gouda Vuurvast AK 70 M Dense Refractory Brick
Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,..
Density 2.55 g/cc
0.0921 lb/in³
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Density 2.55 g/cc
0.0921 lb/in³
Schott B270â„¢ Sheet Glass
B 270â„¢ crown glass in sheet glass form. Manufactured by the up-draw method, offers high stability with respect to solarization in combination with high transmission in the visible wavelength ra..
Density 2.55 g/cc
0.0921 lb/in³
Schott Nextrema® 712-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Density 2.55 g/cc
0.0921 lb/in³
SGL Carbon Group EK 305 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Density 2.55 g/cc
0.0921 lb/in³
Schott N-KZFS2 Glass
Information Provided by SCHOTT North America, Inc.
Density 2.55 g/cc
0.0921 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-..
Density 2.55 g/cc
0.0921 lb/in³
ISO 1183
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding
Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar.
Density 2.55 g/cc
0.0921 lb/in³
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M #11 Filtration Granule (Corona)
3M #11 Filtration Granules are natural minerals used for water filtration in irrigation system.Information provided by 3M
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M #11 Roofing Granule (Corona)
3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M #11 Roofing Granule (Little Rock)
3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M #14 Roofing Granule (Corona)
3M #14 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M #18 Roofing Granule (Corona)
3M #18 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M 7000 Series Copper Roofing Granule (Little Rock)
3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M Blended #11 Blended Roofing Granule (Little Rock)
3M #11 Grade Blended Roofing Granules are combination of ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M Cool Roofing Granule (Corona)
3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products and are designed specifically to have a higher total solar reflectance than standard granu..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M Headlap Roofing Granule (Corona)
3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He..
Density 2.55 - 2.70 g/cc
0.0921 - 0.0975 lb/in³
3M Headlap Roofing Granule (Little Rock)
3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He..
Density 2.55 g/cc
0.0921 lb/in³
Apparent
Gouda Vuurvast SiC 70 Dense Refractory Brick
Description: This type of brick, based on silicon carbide, is because of a very good thermal shock resistance, abrasion resistance and a high thermal conductivity very well suited for waste incinera..