Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0216 g/cc | >= 0.000781 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 33MBHD Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |