Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0216 g/cc | 0.000780 lb/in³ | Expected from single pass expansion |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |
|||
Density | >= 0.0216 g/cc | >= 0.000781 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 33MBHD Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |