Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0340 g/cc | 0.00123 lb/in³ | ISO 845 |
Zotefoams ZOTEK® F 40 HT LS PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Density | 0.0340 g/cc | 0.00123 lb/in³ | ISO 845 |
Zotefoams ZOTEK® F OSU Semi-Rigid PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |
|||
Density | 0.0340 g/cc | 0.00123 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® HL34 Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0340 - 0.0440 g/cc | 0.00123 - 0.00159 lb/in³ | sheet density |
Zotefoams Plastazote® LD38 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |