Zotefoams ZOTEK® F OSU Semi-Rigid PVDF Foam

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Zotefoams
Trade Name ZOTEK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams ZOTEK® F OSU Semi-Rigid PVDF Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.This grade is ideal for soft trim in combination with leathers, textiles and decorative laminates, including low FST cores for composites and divider panels.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0340 g/cc
0.00123 lb/in³
ISO 845
Mechanical Properties Metric English Comments
Tensile Strength 0.417 MPa
60.5 psi
ISO 1798
Elongation at Break 74 %
74 %
Compressive Yield Strength 0.0740 MPa

@Strain 25.0 %
10.7 psi

@Strain 25.0 %
ISO 7214
Tear Strength 0.823 kN/m
4.70 pli
ISO 8067
Compression Set 50 %

@Time 79200 sec,
Strain 50.0 %
50 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; ISO 7214
Thermal Properties Metric English Comments
Thermal Conductivity 0.0321 W/m-K
0.223 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
0.0370 W/m-K
0.257 BTU-in/hr-ft²-°F
mean temp of 50°C; ISO 8301
0.0407 W/m-K
0.282 BTU-in/hr-ft²-°F
mean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 155 °C
311 °F
Descriptive Properties Value Comments
Flammability Heat Release: FAR/CS 25.853, 2 min total
30.2 kWmin/m<sup>2</sup>
Heat Release: FAR/CS 25.853, Peak
35 kW/m<sup>2</sup>at 1 in
Toxic Gas Emission: ABD0031
Pass at 25 mm