Physical Properties Metric English Comments
Density 0.0380 g/cc
0.00137 lb/in³
2 minute residence time pre-expander
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry in..
Density 0.0380 g/cc
0.00137 lb/in³
2.6 minute residence time pre-expander
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry in..
Density 0.0380 - 0.0490 g/cc
0.00137 - 0.00177 lb/in³
sheet density
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0380 - 0.0460 g/cc
0.00137 - 0.00166 lb/in³
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0380 - 0.0460 g/cc
0.00137 - 0.00166 lb/in³
Akzo Nobel Expancel® 551 DE 80 d42 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..