Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0380 g/cc | 0.00137 lb/in³ | 2 minute residence time pre-expander |
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry in.. |
|||
Density | 0.0380 g/cc | 0.00137 lb/in³ | 2.6 minute residence time pre-expander |
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry in.. |
|||
Density | 0.0380 - 0.0490 g/cc | 0.00137 - 0.00177 lb/in³ | sheet density |
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0380 - 0.0460 g/cc | 0.00137 - 0.00166 lb/in³ | |
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0380 - 0.0460 g/cc | 0.00137 - 0.00166 lb/in³ | |
Akzo Nobel Expancel® 551 DE 80 d42 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |