Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0404 - 1.56 g/cc | 0.00146 - 0.0564 lb/in³ | Average value: 0.683 g/cc Grade Count:39 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |