Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.00512 g/cc | 0.000185 lb/in³ | Vapor Density |
Enviro Tech International EnSolv® 5408 n-Propyl Bromide Vapor Degreasing Solvent EnSolv-5408 is the only Boeing approved, stabilized n-Propyl Bromide based solvent for the replacement of Trichloroethylene, Perchloroethylene and 1,1,1-trichloroethane in aerospace vapor degreasing.. |
|||
Density | 0.00512 g/cc | 0.000185 lb/in³ | Vapor Density |
Enviro Tech International EnSolv® n-Propyl Bromide Vapor Degreasing Solvent EnSolv is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane and other hazardous vapor degreasing and general use solvents for critical applications such as oxygen serv.. |
|||
Density | 0.00512 g/cc | 0.000185 lb/in³ | Vapor Density |
Abatron Abosolv™ General Purpose Thinner and Solvent Abosolv™ is a solvent for LiquidWood®: for thinning the product and cleaning up. Abosolv™ can be added to LiquidWood® up to 1 part Abosolv™ to 1 part LiquidWood® by volume. |