Polymer Property : Density = 0.00723 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.160 - 0.200 g/cc
0.00578 - 0.00723 lb/in³
ASTM D792
Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam
CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high..
Density 0.160 - 0.200 g/cc
0.00578 - 0.00723 lb/in³
ISO 845-88
Eurofoam Evacell EVA 200 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Density 0.150 - 0.200 g/cc
0.00542 - 0.00723 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 F-7142 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.