Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.160 - 0.192 g/cc | 0.00578 - 0.00694 lb/in³ | |
Pyrotek C-1 Ceramic fiber paper C-1 Fiberseal paper is a highly uniform paper which assures equal thermal conductivity throughout the product.ApplicationsHigh temperature gaskets Liners Expansion joints Thermal barrier Seals Blast.. |
|||
Density | 0.160 - 0.200 g/cc | 0.00578 - 0.00723 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Sawbones Cellular Rigid Polyurethane Foam 10 pcf Density Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone .. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | Durablanket-S |
Unifrax Anchor-Loc® 2200 Ceramic Fiber Modules The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | |
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | Module |
Unifrax Insulfrax® 1100C Modules Insulfrax® 1100C Modules are a family of high-temperature module products based on Unifrax's Anchor-Loc® attachment systems. Modules used in the Anchor-Loc® systems are constructed with Insulfra.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | |
Unifrax Isofrax® 1260C Paper Fiber Isofrax® 1260C Paper is a unique product which is manufactured by forming Isofrax 1260C Fiber in a nonwoven matrix. The fibers are randomly oriented during manufacture, then held in place with a l.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites RSPA-SOL2 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites RSPA-SOL3 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 1/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.160 - 0.200 g/cc | 0.00578 - 0.00723 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 200 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | |
Unifrax Fiberfrax® 970 Ceramic Fiber Paper 970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. .. |
|||
Density | 0.160 - 0.192 g/cc | 0.00578 - 0.00694 lb/in³ | |
Pyrotek C-1 Fiber Seal Pre-cut Gasket A highly uniform ceramic fiber paper offering even thermal conductivity.Information provided by Pyrotek. |