Polymer Property : Density = 0.00939 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.240 - 0.260 g/cc
0.00867 - 0.00939 lb/in³
Free Density
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.