Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.240 - 0.260 g/cc | 0.00867 - 0.00939 lb/in³ | Free Density |
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |