Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0110 - 0.0200 g/cc | 0.000397 - 0.000723 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 5000 AE Expandable Polystyrene, Standard Flame Retardant Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 10 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type .. |
|||
Density | 0.0110 - 0.0200 g/cc | 0.000397 - 0.000723 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 7000 AE Expandable Polystyrene, Standard Flame Retardant Particle size range is 1.5 - 2.2 mm. Minimum apparent density after two expansions is 10 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l.Processing technology used for Type .. |
|||
Density | 0.0110 - 0.0200 g/cc | 0.000397 - 0.000723 lb/in³ | Density range normally used |
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does.. |
|||
Density | 0.0110 - 0.0200 g/cc | 0.000397 - 0.000723 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0110 - 0.0200 g/cc | 0.000397 - 0.000723 lb/in³ | |
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **) Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Density | 0.0110 - 0.0200 g/cc | 0.000397 - 0.000723 lb/in³ | |
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **) Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7.. |
|||
Density | >= 0.0110 g/cc | >= 0.000397 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Styrocell® B733A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the .. |
|||
Density | >= 0.0110 g/cc | >= 0.000397 lb/in³ | Minimum apparent density on a continuous pre-expander after two expansions |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |