Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.304 g/cc | 0.0110 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.304 g/cc | 0.0110 lb/in³ | ASTM D1056 |
Rogers Corporation Bisco® L3 Premiere Next Generation Dynamic Flooring Material BISCO® L3 Premiere silicone foam technology is the next generation in dynamic and floating floor materials from Rogers Corporation developed specifically to meet the most challenging global require.. |