Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0166 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.460 g/cc
0.0166 lb/in³
tap; ASTM D4164
Proto3000 CastForm™ PS Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Directly produce complex investment casting patterns without tooling..Features: Functions like foundry wax and is “foundry friendly”Low residual ash content (less than 0.02%)Short bur..
Density 0.460 g/cc
0.0166 lb/in³
Saint-Gobain Chemfab® TCK® 1589 High-Strength Plain Weave Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Density 0.460 g/cc
0.0166 lb/in³
ISO 1183
Stir SpA POROCELL Z 545 ATS (PVC)
Application: Matt super foam for injection moldingInformation provided by STIR SpA
Density 0.460 g/cc
0.0166 lb/in³
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE
ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped ..
Density 0.460 - 0.520 g/cc
0.0166 - 0.0188 lb/in³
ISO 1183
Fainplast Compounds EVAtech 805S Ethylene Vinyl Acetate Foam
EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds
Density 0.460 g/cc
0.0166 lb/in³
Typical, 3M QCM 14.24.6
3M HGS6000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.460 g/cc
0.0166 lb/in³
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.460 g/cc
0.0166 lb/in³
3M K46 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..