Physical Properties Metric English Comments
Density 0.460 - 0.520 g/cc
0.0166 - 0.0188 lb/in³
ISO 1183
Fainplast Compounds EVAtech 805S Ethylene Vinyl Acetate Foam
EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds
Density 0.480 - 0.520 g/cc
0.0173 - 0.0188 lb/in³
True, 3M QCM 14.24.6
3M H50/10000EPX Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..