Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0270 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0270 - 0.0370 g/cc
0.000975 - 0.00134 lb/in³
sheet density
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0270 - 0.0370 g/cc
0.000975 - 0.00134 lb/in³
sheet density
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0270 - 0.0360 g/cc
0.000975 - 0.00130 lb/in³
sheet density
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0270 - 0.0350 g/cc
0.000975 - 0.00126 lb/in³
sheet density
Zotefoams Plastazote® LD33LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0270 g/cc
0.000975 lb/in³
Core Density, ASTM D3574
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 0.0270 - 0.0330 g/cc
0.000975 - 0.00119 lb/in³
Akzo Nobel Expancel® 091 DE 80 d30 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0270 - 0.0330 g/cc
0.000975 - 0.00119 lb/in³
Akzo Nobel Expancel® 091 DE 40 d30 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0270 - 0.0350 g/cc
0.000975 - 0.00126 lb/in³
sheet density
Zotefoams Plastazote® LD34 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..