Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0312 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.863 g/cc
0.0312 lb/in³
ASTM D1505
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid)
A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne
Density 0.863 - 0.872 g/cc

@Temperature 70.0 °C
0.0312 - 0.0315 lb/in³

@Temperature 158 °F
Kazanorgsintez Cosintol 242
Production Method: Mixture of polyoxyethylated esters of higher fatty alcohols C12-C14 fractions. Applications: Intended for use as an effective nonionic surface-active substance in the production o..
Density 0.863 - 0.887 g/cc
0.0312 - 0.0320 lb/in³
Lord Adhesives 459T Toluene Adhesion Promoter for Lord Acrylic, Epoxy, Urethane and Cyanoacrylate Adhesives
To meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surface modifiers. Lord® Adhesion Enhancers..
Density 0.863 - 0.899 g/cc
0.0312 - 0.0325 lb/in³
Lord Adhesives AP-134 Reactive Polymer Primer or Adhesive for Polar Substrates
Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa..
Density 0.863 - 0.899 g/cc
0.0312 - 0.0325 lb/in³
Lord Adhesives Chemlok® AP-134 One-Coat Primer
Chemlok® AP-134 is a clear, low viscosity, solventborne reactive primer which can function as a primer or adhesive for a variety of polar substrates. Substrates include: steel, aluminum, brass, E..
Density 0.863 g/cc

@Temperature 20.0 °C
0.0312 lb/in³

@Temperature 68.0 °F
LyondellBasell TBAcâ„¢ Solvent, Tertiary butyl acetate
Information provided by Lyondell.
Density 0.865 g/cc
0.0312 lb/in³
Fired Density at 2300°F
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 0.863 g/cc
0.0312 lb/in³
ConocoPhillips Syncon® 68 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Density 0.863 g/cc
0.0312 lb/in³
ELM® Bar & Chain Lubricant Biodegradable –Biobased Bar & Chain Lube
Description: ELM Biotechbased™ Bar & Chain Oil is a high quality biodegradable bar and chain saw lubricant formulated with the best optimized biotechnology using USA-grown natural seed oil that sur..
Density 0.863 g/cc

@Temperature 15.0 °C
0.0312 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Mobil 1 75W-140 Gear Lubricant LS
Mobil 1 Synthetic Gear Lubricant LS 75W-140 is a supreme performance, synthetic, multi-purpose, automotive gear lubricant designed to meet the highest level performance requirements of many modern p..
Density 0.864 g/cc
0.0312 lb/in³
ASTM D792
Dow Engage® 8130 Polyolefin Elastomer
Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process..
Density 0.863 g/cc
0.0312 lb/in³
ASTM D792
Dow Engage® 8180 Polyolefin Elastomer
Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w..
Density 0.863 g/cc
0.0312 lb/in³
ASTM D792
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer
Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification...
Density 0.865 g/cc
0.0312 lb/in³
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact
These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou..
Density 0.863 g/cc
0.0312 lb/in³
ConocoPhillips Hydroclear® 250 Industrial Oil
Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende..
Density 0.863 g/cc
0.0312 lb/in³
ConocoPhillips Hydroclear® 32 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
Density 0.863 g/cc

@Temperature 15.0 °C
0.0312 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Mobil 1 75W-140 Gear Lubricant LS
Mobil 1 Synthetic Gear Lubricant LS 75W-140 is a supreme performance, synthetic, multi-purpose, automotive gear lubricant designed to meet the highest level performance requirements of many modern p..
Copyright © lookpolymers.com All Rights Reserved