Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.888 g/cc @Temperature 20.0 °C |
0.0321 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell THF Tetrahydrofuran Information provided by Lyondell. |
|||
Density | 0.889 g/cc @Temperature 15.0 °C |
0.0321 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil 150 Exxon Sawguide Oil EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi.. |
|||
Density | 0.888 g/cc @Temperature 15.0 °C |
0.0321 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 18M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.889 g/cc @Temperature 15.0 °C |
0.0321 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 30 1630 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.888 g/cc | 0.0321 lb/in³ | Exxon Method |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Density | 0.888 g/cc | 0.0321 lb/in³ | Exxon Method |
ExxonMobil EXACT™ 4053 Plastomer for Film Applications Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Density | 0.888 g/cc @Temperature 15.0 °C |
0.0321 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 18M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.889 g/cc @Temperature 15.0 °C |
0.0321 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil 150 Exxon Sawguide Oil EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi.. |
|||
Density | 0.889 g/cc @Temperature 15.0 °C |
0.0321 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 30 1630 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.888 g/cc | 0.0321 lb/in³ | |
ConocoPhillips Hydroclear® 320 Multipurpose R&O Oil, AGMA Lubricant No. 6 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Density | 0.888 g/cc | 0.0321 lb/in³ | |
ConocoPhillips Hydroclear® 320 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |