ExxonMobil EXACT™ 4053 Cast Plastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXACT™ 4053 Cast Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with polyolefines to improve the heat sealing performance and/or toughness in film applications. Exact 4053 contains no antioxidants. Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications:Blend PartnerCast Film Data provided by the manufacturer, Exxon Chemical
Physical Properties Metric English Comments
Density 0.888 g/cc
0.0321 lb/in³
Exxon Method
Melt Flow 2.2 g/10 min
2.2 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 4.34 MPa
630 psi
ASTM D882
Film Tensile Strength at Yield, TD 3.24 MPa
470 psi
ASTM D882
Film Elongation at Break, MD 440 %
440 %
ASTM D882
Film Elongation at Break, TD 820 %
820 %
ASTM D882
Film Elongation at Yield, MD 10 %
10 %
ASTM D882
Film Elongation at Yield, TD 10 %
10 %
ASTM D882
Puncture Energy 6.21 J
4.58 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 30 g
30 g
ASTM D1922
Elmendorf Tear Strength TD 90 g
90 g
ASTM D1922
Dart Drop Test 120 g
0.265 lb
ASTM D1709A
Film Tensile Strength at Break, MD 64.8 MPa
9400 psi
ASTM D882
Film Tensile Strength at Break, TD 46.2 MPa
6700 psi
ASTM D882
1% Secant Modulus, MD 36.5 MPa
5300 psi
ASTM D882
1% Secant Modulus, TD 35.9 MPa
5200 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 70.0 °C
158 °F
Exxon Method
Vicat Softening Point 133 °C
271 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 0.50 %
0.50 %
ASTM D1003
Gloss 89 %
89 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 15 lbf
ExxonMobil Method