Polymer Property : Density = 0.03739 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.035 g/cc
0.03739 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP MFB22S PP
LNP* THERMOCOMP* MFB22S is a compound based on Polypropylene containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Heat Stabilized.
Density 1.035 g/cc
0.03739 lb/in³
ASTM D792
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Density 1.035 g/cc
0.03739 lb/in³
ASTM D792
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Density 1.035 g/cc
0.03739 lb/in³
ASTM D792
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.