Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.035 g/cc
0.03739 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 58
58
ASTM D785
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 86.02 MPa
12480 psi
ASTM D790
Flexural Modulus 4.30 GPa
624 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Gardner Impact 0.500 J
0.369 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ASTM D648
Flammability, UL94 HB
HB