Physical Properties Metric English Comments
Density 1.052 g/cc
0.03801 lb/in³
ASTM D792
North Wood Plastics 60 PP + UNIFILL (40% Wood Fiber)
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It..