Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.052 g/cc | 0.03801 lb/in³ | ASTM D792 |
North Wood Plastics 60 PP + UNIFILL (40% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |