Physical Properties Metric English Comments
Density 1.106 g/cc
0.03996 lb/in³
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing..
Density 1.106 g/cc
0.03996 lb/in³
ISO 1183
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..