Material Notes:
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).ApplicationsTX is used for:flat display substratesoptical componentsmiscellaneous goods.TP/TH are used for:food package sheeting as well as in manufacturingelectronic equipment and componentsmiscellaneous goodsTE/CL are for:electronic equipment and componentsinformation equipment componentsAV equipment, etc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Density 1.106 g/cc
0.03996 lb/in³
ISO 1183
Melt Flow 2.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
33 g/10 min

@Load 10.0 kg,
Temperature 220 °C
33 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 57
57
ISO 2039-2
Tensile Strength at Break 34.0 MPa
4930 psi
50mm/min; ISO 527-2
39.0 MPa
5660 psi
50mm/min; ASTM D638
Elongation at Break 50 %
50 %
50mm/min; ISO 527-2
Flexural Strength 73.0 MPa
10600 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2mm/min; ISO 178
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179-2
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ISO 75-2
81.0 °C
178 °F
ASTM D648
Vicat Softening Point 94.0 °C
201 °F
50N; ISO 306
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 2.0 %

@Thickness 2.00 mm
2.0 %

@Thickness 0.0787 in
ISO 14782
Transmission, Visible 91 %

@Thickness 2.00 mm
91 %

@Thickness 0.0787 in
ISO 13468-1
Users viewing this material also viewed the following: