Density 1.21 - 1.222 g/cc
0.0437 - 0.04415 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DX99620C PC
LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.