Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.634 g/cc | 0.05903 lb/in³ | |
Pyrotek TS-235 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek. |