Polymer Property : Density = 1.634 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.634 g/cc
0.05903 lb/in³
Pyrotek TS-235 Thermoset Electrical Insulation Product
Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek.