Physical Properties Metric English Comments
Density 0.0230 - 0.0600 g/cc
0.000831 - 0.00217 lb/in³
Pressurized batch pre-foamer; Usual Use
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr..
Density 0.0230 - 0.0600 g/cc
0.000831 - 0.00217 lb/in³
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene  (discontinued **)
Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi..
Density 0.0220 - 0.0600 g/cc
0.000795 - 0.00217 lb/in³
Polimeri Europa Extir® P 1212 Expandable Polystyrene  (discontinued **)
Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. ..
Density 0.0220 - 0.0600 g/cc
0.000795 - 0.00217 lb/in³
Density range normally used
Polimeri Europa Extir® P 1212 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.2 - 0.5 mm. Minimum apparent density on a discontinuous pre-expander is 21 g/l. Minimum apparent density on a continuous pre-expander is 25 g/l.Processing technology used ..
Density 0.0400 - 0.0600 g/cc
0.00145 - 0.00217 lb/in³
ISO 845-88
Eurofoam Evacell EVA 50/S EVA + NR Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..