Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Extir® E 2000 AE Expandable Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Extir® E 2000 AE Expandable Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade is used for the very fast cycle production of thin section contour mouldings with a medium to very high density. It shows a very short maturing time, even at very high density, an excellent moulding processability, a good fusion, a good surface aspect and a very good dimensional stability.Applications: Extir E 2000 AE is used mainly in thin section, medium / high density packaging where, for legislative or safety reasons, the use of a flame retardant material is required. Typical applications are: • thin section packaging (from 5 to 10 mm) • decorative ceiling panels • baby/child safety seatIt is recommended to keep the product in a dry well ventilated store between 15-20°C. For product packaged in octabins the guaranteed shelf-life is one month; product in steel drums has a six months guaranteed shelf-life. During the processing of Expandable Polystyrene any sparkle or flame must be avoided and smoking should be forbidden. An adequate electrical grounding of machinery and of pneumatic transport lines is recommended. For further information concerning storage, packaging and processing precautions please refer to "Styrenics - Technical data sheets" and to the "Extir Safety Data Sheet". Regarding "flame retardant" properties, articles made from Extir AE are officially certified “B1 nach DIN 4102”. The action of the flame retardant additive is exerted only after the elimination of blowing agent and, therefore, only after Extir AE has been transformed into foamed articles (suitably aged where necessary).Processing: Extir E 2000 AE can be easily pre-expanded on conventional equipment over a wide density range (from 22 to 60 kg/m³), despite its low pentane content. This product needs minimum maturation times (from 1 to 48 hours), even at high density. Moreover the steaming cycle is nearly not influenced by the maturation time. Due to excellent processability and low pentane content, it is possible to operate with very fast cycle times (mainly by reducing the cooling times) and with low steam pressures. Moulded items exhibit a very high fusion level, excellent surface finishing, good mechanical properties and an excellent dimensional stability. Extir E 2000 AE can be moulded on all types of shape moulding machines.Information provided by Polimeri Europa
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density 0.0230 - 0.0600 g/cc
0.000831 - 0.00217 lb/in³
Apparent Bulk Density 0.0220 g/cc
0.000795 lb/in³
On a discontinuous pre-expander
0.0240 g/cc
0.000867 lb/in³
On a continuous pre-expander after one expansion
Particle Size 400 - 750 µm
400 - 750 µm
Users viewing this material also viewed the following: