Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8599 BLK TPE compound for acoustic barrier applications requiring high density. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cookson Group Plaskon® 3400 Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cookson Group Plaskon® S-7S Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
SGL Carbon Group EK 2201 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C30 S006 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C30 S012 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.82 g/cc @Temperature 25.0 °C |
0.0658 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Density | 1.82 g/cc @Temperature 25.0 °C |
0.0658 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® LS230 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Plenco 7556 Phenolic, Briquette, Injection Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Toho Tenax Besfight® G60-600 12K UMA-5C A303 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ISO 1183 |
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ISO 1183 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.Information supplied by Sumitomo Bak North America. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.82 - 1.86 g/cc | 0.0658 - 0.0672 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 75-2 Linear Low Density Polyethylene, 75% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Dry As Molded |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |