Polymer Property : Density = 0.0697 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.93 g/cc
0.0697 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o..
Density 1.93 g/cc
0.0697 lb/in³
DIN 53 47
Albis Plastics Tedur® L 9521-1 PPS, 60% Glass Fiber/Mineral  (discontinued **)
Extremely Rigid. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Sockets, Plugs and HandlesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperatur..
Density 1.93 g/cc
0.0697 lb/in³
IDI Composites 48-50 Thermoset Polyester, Molding
Moderate strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer.
Density 1.93 g/cc
0.0697 lb/in³
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Density 1.93 g/cc
0.0697 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® AD 60 Perfluoropolymer
Hyflon® AD 60 is an amorphous perfluoro-polymer available in powder form.Hyflon® AD polymers resemble semicrystalline perfluoropolymers in their performance properties as they exhibit high tem..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF080 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF085 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF090 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF095 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF100 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF105 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF110 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 025 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 050 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 100 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 175 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 250 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 300 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 g/cc
0.0697 lb/in³
ASTM D792
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF115 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 075 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 200 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 g/cc
0.0697 lb/in³
ASTM D792
Plenco 08225 Polyester BMC, Compression Molded
PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert..
Density 1.93 g/cc
0.0697 lb/in³
Trelleborg Emerson & Cuming Stycast® E-1030 One-Component Epoxy Low Stress Encapsulant
Emerson & Cuming E-1030 Stycast® One-Component Epoxy Low Stress EncapsulantDesigned for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low te..
Density 1.93 g/cc
0.0697 lb/in³
DIN 53 47
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral
Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting..
Density 1.93 g/cc
0.0697 lb/in³
Molded
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 150 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..