Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.84 - 2.04 g/cc | 0.0665 - 0.0737 lb/in³ | Molded |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Density | 1.84 - 2.04 g/cc | 0.0665 - 0.0737 lb/in³ | Molded |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |