Bulk Molding Compounds BMC A30 General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC A30 General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression molding.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.84 - 2.04 g/cc
0.0665 - 0.0737 lb/in³
Molded
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength 33.1 - 46.9 MPa
4800 - 6800 psi
Flexural Strength 82.7 - 110 MPa
12000 - 16000 psi
Flexural Modulus 6.89 - 8.27 GPa
1000 - 1200 ksi
Compressive Strength 93.1 - 121 MPa
13500 - 17500 psi
Izod Impact, Notched 1.60 - 3.20 J/cm
3.00 - 6.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
This material is not UL listed.
Electrical Properties Metric English Comments
Dielectric Strength 10.8 - 12.8 kV/mm
275 - 325 kV/in
short time
Arc Resistance >= 180 sec
>= 180 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F