Physical Properties Metric English Comments
Density 2.071 g/cc
0.07482 lb/in³
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) ..
Density 2.071 g/cc
0.07482 lb/in³
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..
Density 2.071 g/cc
0.07482 lb/in³
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are..