Polymer Property : Density = 0.076 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.1 g/cc
0.076 lb/in³
Relative Density; ASTM D792
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound
Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information ..