Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.23 g/cc | 0.0806 lb/in³ | ASTM D792 |
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
ITW Devcon Metal Repair Bronze Putty (BR), Bronze Information provided by ITW Devcon |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey Information provided by ITW Devcon |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
Ferro F 2719 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals.. |
|||
Density | 2.23 - 2.25 g/cc | 0.0806 - 0.0813 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
Density | 2.23 g/cc @Temperature 25.0 °C |
0.0806 lb/in³ @Temperature 77.0 °F |
|
Schott DURAN® Borosilicate Glass Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, general-purpose glass for apparatus for the chemical industry, for pipelines, and glasswareInformation provided by.. |
|||
Density | 2.23 g/cc @Temperature 25.0 °C |
0.0806 lb/in³ @Temperature 77.0 °F |
|
Schott DURATAN® Borosilicate Glass Prestressed borosilicate glass 3.3, chemically and thermally highly resistant, Flameproof lighting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below .. |
|||
Density | 2.23 g/cc @Temperature 25.0 °C |
0.0806 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8347 Borosilicate Glass Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, highly UV-transmitting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium i.. |
|||
Density | 2.23 g/cc @Temperature 25.0 °C |
0.0806 lb/in³ @Temperature 77.0 °F |
|
Schott KIMAX® Borosilicate Glass Laboratory Glass Drainline from Borosilicate glass 3.3. Chemically and thermally highly resistant.The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10.. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | Real Density |
SGL Carbon Group CF 480 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM 0223 B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | ASTM D792 |
Saint-Gobain Fluoroloy® A15 High Performance Seal Material Improved sealing at low pressure; Can be abrasive running against soft metals
Information provided by Saint-Gobain Performance Plastics. |
|||
Density | 2.23 g/cc @Temperature 25.0 °C |
0.0806 lb/in³ @Temperature 77.0 °F |
|
Schott BORO-8330â„¢ Borosilicate Glass Borosilicate glass 3.3 acc. ISO 3585, chemically highly resistant, highly resistant to thermal shock, special applications in the pharmaceutical industryInformation provided by SCHOTT AG. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
Schott BOROFLOAT® Borosilicate Float Glass This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro.. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
Devcon Combo Wear FC Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | ASTM D792 Method A |
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe.. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | ASTM D792 Method A |
Arlon DiClad 880 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.23 g/cc | 0.0806 lb/in³ | |
Corning Pyrex® 7740 Borosilicate Glass Pyrex® sheet provides unique chemical, thermal, mechanical, and optical properties. Available in thicknesses from 3/32 inches to 2.25 inches. Tempering increases temperature and pressure capabili.. |
|||
Density | 2.23 g/cc @Temperature 25.0 °C |
0.0806 lb/in³ @Temperature 77.0 °F |
|
Schott CONTURAX® Borosilicate Glass Borosilicate glass tubing and rod, varying types of inner and outer shapes Lighting, giftware, and decoration The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |